Default orange peel

I cant get rid of the orange peel- I have tried everything- please help! I have the caswell adjustable gun 30-50 kv one. Any help would be terrific!
Reply With Quote
  #2 (permalink)  
Old 05-04-2008, 12:32 AM
mikmj's Avatar
Amateur Metal Finisher
 
Join Date: Aug 2005
Location: KY.
Posts: 59
mikmj
Default Re: orange peel

Quote:
Originally Posted by ryandayonftrp View Post
I cant get rid of the orange peel- I have tried everything- please help! I have the caswell adjustable gun 30-50 kv one. Any help would be terrific!

Got pics......
__________________
Mike

MJM Powder Coating
Reply With Quote
  #3 (permalink)  
Old 05-04-2008, 03:20 PM
Newbie
 
Join Date: Dec 2006
Posts: 37
powdersparky is an unknown quantity at this point
Default Re: orange peel

What are you powdercoating? More details and the info will hopefully follow.
Reply With Quote
  #4 (permalink)  
Old 05-05-2008, 06:18 PM
Newbie
Caswell Platinum Member
 
Join Date: Feb 2008
Posts: 12
djgold4653 is on a distinguished road
Default Re: orange peel

orange peel usually means powder too thick
Reply With Quote
  #5 (permalink)  
Old 05-08-2008, 05:16 PM
nuttyman's Avatar
Metal Finishing Guru
 
Join Date: Sep 2003
Location: Rio Rancho, NM
Posts: 553
nuttyman
Default Re: orange peel

wet sand it & buff it--you'll get rid of it that way!
__________________
SouthWest Powderworx
Tyler Nutter
5054803934
www.swpowder.com
myspace/swpowder
tyler@swpowder.com
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Less orange peel NXGHOST Powder Coating Questions 4 03-28-2007 04:43 PM
Orange Peel? squaredealer Metal Polishing Questions 3 09-10-2004 09:46 AM
Orange Peel ke4ram Powder Coating Questions 3 06-07-2004 11:29 AM
Orange Peel griffsfsr Powder Coating Questions 5 03-02-2004 11:24 AM
Orange peel esahlin Powder Coating Questions 5 09-04-2003 12:50 AM


All times are GMT -4. The time now is 05:25 AM.


Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.