Default Thank You Ken Hill for the Inspiration

So a few months ago as I was browsing ColumbiaCoatings I noticed one of the customers examples. which was a gold vein base with a Candy Red on top.

So I ordered some Gold Vein and felt like experimenting on my Honda ecu. I must say Im VERY HAPPY.

Heres the example.

http://store.columbiacoatings.com/pr...6024_image.jpg




Heres mine.



Reply With Quote
  #2 (permalink)  
Old 05-07-2008, 09:47 PM
JTW37's Avatar
Experienced Metal Finisher
Caswell Platinum Member
 
Join Date: Feb 2006
Location: Bristol, In
Posts: 448
JTW37 is an unknown quantity at this point
Default Re: Thank You Ken Hill for the Inspiration

I Like! Looks pretty good to me. I need to give some of that a try.
__________________
Who says you can't teach an ole dog new tricks?
Reply With Quote
  #3 (permalink)  
Old 05-07-2008, 11:22 PM
Newbie
 
Join Date: Dec 2007
Location: Buffalo
Posts: 35
95gts is on a distinguished road
Default Re: Thank You Ken Hill for the Inspiration

great job, looks like a nice deep color
Reply With Quote
  #4 (permalink)  
Old 05-08-2008, 12:11 PM
Newbie
 
Join Date: May 2007
Posts: 49
GCPJohn is on a distinguished road
Default Re: Thank You Ken Hill for the Inspiration

Very cool. I've heard of using the silver vein with a candy top coat, but not gold vein...looks great!
Reply With Quote
  #5 (permalink)  
Old 05-08-2008, 07:58 PM
Newbie
 
Join Date: Sep 2007
Posts: 15
pumaking is on a distinguished road
Default Re: Thank You Ken Hill for the Inspiration

Would adding another layer of Candy on top make it brighter or darker?
Reply With Quote
  #6 (permalink)  
Old 05-09-2008, 05:26 PM
Newbie
 
Join Date: May 2007
Posts: 49
GCPJohn is on a distinguished road
Default Re: Thank You Ken Hill for the Inspiration

Darker. More coats means the light has to penetrate said extra coats, making it darker.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off


All times are GMT -4. The time now is 05:22 AM.


Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.