Old 05-17-2003, 11:51 PM
Experienced Metal Finisher
 
Join Date: Dec 2002
Location: Central New York
Posts: 353
DALE will become famous soon enough
Default

regular elements will work for your application. and wiring sounds like you got it. Now the advice will be $7995.00 and you still saved 5 bucks versus the $8000 oven.
Reply With Quote
  #12 (permalink)  
Old 05-18-2003, 11:07 AM
getastro's Avatar
Amateur Metal Finisher
 
Join Date: May 2003
Location: NSB, FL.
Posts: 59
getastro
Default oven

Thanks Dale for all the info. Just drawing plans up now for the oven frame. The info you gave is just what I was looking for. Also the check is in the mail.
P.S. When you hook up your elements to the relay, do you hook up both the red & black wire (for 220V) to thr relay or one to the elements the other to the relay?
Reply With Quote
  #13 (permalink)  
Old 05-18-2003, 11:40 PM
Experienced Metal Finisher
 
Join Date: Dec 2002
Location: Central New York
Posts: 353
DALE will become famous soon enough
Default

relays vary from type to type. I prefer ones that open all lines. Never tried any other. Mine has both on relay then to element.then next element to previous one and so on.
Reply With Quote
  #14 (permalink)  
Old 05-18-2003, 11:56 PM
getastro's Avatar
Amateur Metal Finisher
 
Join Date: May 2003
Location: NSB, FL.
Posts: 59
getastro
Default oven

Thanks, I guess I have to go out and start to order stuff. Thanks a lot Dale.
Reply With Quote
  #15 (permalink)  
Old 07-26-2003, 02:33 AM
warchild's Avatar
Amateur Metal Finisher
 
Join Date: Feb 2003
Location: Seymour,Tn.
Posts: 147
warchild
Default Ovens

If anyone wants a BIG oven you can check out this site. www.equipmentresale.com they have some big used 6ft x 5ft x 6ft ovens for $1,500. some in rough condition. and they have IR ovens up to 14ft long too.
__________________
WARCHILD
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
powder coating over powder coat? corybarta Powder Coating Questions 6 08-21-2006 09:15 AM
where to buy a real powder coating oven? randygrapes218 Powder Coating Questions 2 08-15-2004 12:50 AM
Powder coating oven suggestion (wiring) tomg552001 Oven Building Forum 1 04-22-2004 02:02 PM
Non-paint powder coating dshepherd Powder Coating Questions 6 01-26-2004 12:49 PM
powder coating oven tougher finish required d608454 Powder Coating Questions 5 07-27-2003 10:07 PM


All times are GMT -4. The time now is 08:01 PM.


Powered by vBulletin® Version 3.7.4
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0
Copyright © Caswell Inc.