Default Re: Does anyone use IRON PHOSPHAT??

Thanks for the welcome Harleydad. Is your name Harley
Reply With Quote
  #12 (permalink)  
Old 06-27-2008, 03:22 PM
Harleydad's Avatar
Metal Finishing Guru
 
Join Date: Dec 2006
Location: Wisconsin
Posts: 573
Harleydad is an unknown quantity at this point
Default Re: Does anyone use IRON PHOSPHAT??

Quote:
Originally Posted by Powder_Coating_Pros View Post
Now thats what I am talking about!
No kidding, damb thats large.

Blazin, do you use surcoat 915 or something else? Is it a no rinse? Do you titrate?
Reply With Quote
  #13 (permalink)  
Old 06-27-2008, 05:41 PM
Newbie
 
Join Date: Jun 2008
Posts: 23
JollyCoat is on a distinguished road
Default Re: Does anyone use IRON PHOSPHAT??

there is a one step dry in place phosphate from PBTP
Reply With Quote
  #14 (permalink)  
Old 06-27-2008, 06:35 PM
Amateur Metal Finisher
 
Join Date: Jul 2007
Location: BC, Canada
Posts: 66
Blazin_Jason is an unknown quantity at this point
Default Re: Does anyone use IRON PHOSPHAT??

We use a an iron phosphate from Henkel, it's rinsed afterwards just with fresh water. We also use a product for items that are too large to fit into the tanks using a hot water pressure washer.
Reply With Quote
  #15 (permalink)  
Old 07-19-2008, 12:32 PM
Metal Finishing Guru
 
Join Date: Jun 2006
Posts: 613
Banditperformance is on a distinguished road
Default Re: Does anyone use IRON PHOSPHAT??

Im trying Liquiguard PC right now. Its a dry in place Pretreatment. So far I got a sample, tried it on my Sled parts, Lollypop red over ground metal. Liquiguard never changed the color of the bare metal, and the powder is holding up to snow, ice and tree's so far
Now waiting on 2 gallons. Seems shipping is taking forever
__________________
Dan Pesonen
Bandit Powder Coat <<From Powder to Perfection>>
Forest Grove, BC Canada

Personal motto:
"If it ain't broke, modify somethin till it is"
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Iron Plating wreini Services Offered/Wanted 4 06-07-2008 11:47 PM
Iron Phosphate? Inferno Powder Coating Questions 2 02-25-2006 08:32 PM
cast iron traciej68 Other Metal Finishing Questions 3 08-27-2005 01:26 AM
cast iron traciej68 Electroplating Questions 1 10-12-2004 07:46 PM
Iron L98-Z Metal Polishing Questions 1 02-20-2002 01:19 AM


All times are GMT -4. The time now is 04:20 PM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.