I see ****wood selling it. I don't see it in Tiger or DuPont's selections.
Anyone know? I'd really like to have it on-hand at the shop.
Thanks!
I see ****wood selling it. I don't see it in Tiger or DuPont's selections.
Anyone know? I'd really like to have it on-hand at the shop.
Thanks!
I believe NIC (Prismatic Powders) has one as does Powder Buy the Pound.
Powder Buy The Pound
Please don't be fooled by marketing ploys - there is no such thing as single stage chrome powder.
All chrome powders can be used as a single stage - but they lack proper UV protection and WILL oxidize over time.
If you look at the web site referenced in the last post, they recommend putting a clear coat over their "single stage". How can you call a powder "single stage" and yet recommend that you clear itIt's marketing jargon, and it's deceptive.
All metallic powders should be clear coated for best results and durability. The metallic flake in these powders corrodes if it's not protected.
Caveat emptor!
--
Lance Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Please support the moderators on our site by leaving reputation for their helpful posts. Read more here.
yeah, I saw that side note later. Pretty lame, thanks guys!
NIC also recommends a clear.
when you say clear coat what method do you mean?
regular old fashion compressor and paint gun with liquid clear coating paint?
Best regards
atheos_mb
I am just getting into powder coating and need some help.
Just courous as to what is the most durable clear coat to use on the caswell extreme chrome powder.
I just ordered the extreme chrome and didn't know at the time that I needed clear.