  #1 (permalink)  
Old 06-01-2003, 10:17 PM
Amateur Metal Finisher
 
Join Date: May 2003
Posts: 162
Fireblade
Default Manufacturer of Powder from Caswell and Hotcoat

Does anyone know the manufacturer of the powders sold by Caswell and by Hotcoat? I need some more detailed information concerning these brands of powders, and the people at Hotcoat are kinda useless at the answers. I have not questioned Caswell yet, so employees of Caswell, disregard the useless part
Reply With Quote
  #2 (permalink)  
Old 06-02-2003, 11:36 AM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,356
Blog Entries: 1
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default

What info do you need? We'll probably be able to get it for you.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote
  #3 (permalink)  
Old 06-05-2003, 08:54 PM
Amateur Metal Finisher
 
Join Date: May 2003
Posts: 162
Fireblade
Default

Ok, how bout some colors which are outgassing formulas?
Reply With Quote
  #4 (permalink)  
Old 06-05-2003, 10:09 PM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,356
Blog Entries: 1
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default

Sorry, I don't understand what you're looking for?

We can get technical data sheets on any of our colors and will gladly share that info.

We buy all our powders from HB Fuller in bulk, which allow us to pass on savings and their technical expertise to our customers.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote
  #5 (permalink)  
Old 06-09-2003, 11:57 AM
Amateur Metal Finisher
 
Join Date: May 2003
Posts: 162
Fireblade
Default

Outgassing formulas basically allow the trapped gasses in a casting to escape through the powdercoating surface easier, allowing a much smoother finish. Kinda like fisheyes in a painted surface, you can add fish eye eliminator to help prevent this from happening, only it is made into the powdercoating itself, not added by the end user, or as far as I know it is not.
Reply With Quote
  #6 (permalink)  
Old 06-11-2003, 11:29 AM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,356
Blog Entries: 1
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default

We asked our supplier about this and yes, they do offer some products with outgassing formulas. Was there a specific color you wanted? What quantity did you need?

The two they mentioned to us were both TGIC black colors that we don't currently stock.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off


All times are GMT -4. The time now is 09:43 AM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.