Default "Bronze" powder coating

A woman from NYC contacted me. She has about 80 assemblies used to hang mannequins from. They consist of tubing, wire forms, and a cast iron base... among other miscellaneous parts maybe. They are all polished. She would like them to be powder coated "bronze".
I don't like to turn work away, but this is not my "forte". I do mostly functional coatings and only dabble in the very pretty things for my own (or friends') enjoyment. I figured that some of you on here would be the perfect coaters to help this woman.
If anyone is interested, please send me your contact info, and I will forward it to her.

chris@precisioncoatingtech.com

Thanks.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Single-stage "Chrome" powder, who makes it? HardShell Powder Coating Questions 12 11-17-2008 10:43 AM
Powder match for "chassis black"? swpruett Powder Coating Questions 0 04-23-2008 11:45 AM
Caswell's "Tinted Brass" and "Candy Gold " autoshopowner Powder Coating Questions 15 05-18-2007 08:45 AM
"Buffing out" powder coat - possible?? skiddz Powder Coating Questions 4 03-03-2004 01:20 AM
"Hard" Anodizing vs. "normal"; differenc dagobert Anodizing Questions 6 02-27-2004 12:24 AM


All times are GMT -4. The time now is 07:33 PM.


Powered by vBulletin® Version 3.7.4
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0
Copyright © Caswell Inc.