    Question 100% Gloss Clear over 60% Gloss Powder...

    Was wondering if any of you guys have done this...

    Extreme or 100% Gloss Clear over a 60% Gloss powder??

    The reason I ask is because i have been having really good luck (knock on wood) with the 60% Black w/ outgassing additive already in it. I have a ton of customers that want Gloss Black. What will the 60% Black look like with 100% clear on top of it?? Good?? Like regular 100% gloss black?
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  2. #2
    Join Date
    Jul 2008
    Location
    Garland, TEXAS
    Posts
    636

    Default Re: 100% Gloss Clear over 60% Gloss Powder...

    Quote Originally Posted by wetdream View Post
    Was wondering if any of you guys have done this...

    Extreme or 100% Gloss Clear over a 60% Gloss powder??

    The reason I ask is because i have been having really good luck (knock on wood) with the 60% Black w/ outgassing additive already in it. I have a ton of customers that want Gloss Black. What will the 60% Black look like with 100% clear on top of it?? Good?? Like regular 100% gloss black?
    I do that with several colors I have. Works great.
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  3. #3
    Join Date
    Feb 2008
    Posts
    63

    Default Re: 100% Gloss Clear over 60% Gloss Powder...

    And this will be ok with a powder that has a Outgassing additive in it?? The 60% that I use comes with this already in it??
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  4. #4
    Join Date
    Jul 2008
    Location
    Garland, TEXAS
    Posts
    636

    Default Re: 100% Gloss Clear over 60% Gloss Powder...

    Quote Originally Posted by wetdream View Post
    And this will be ok with a powder that has a Outgassing additive in it?? The 60% that I use comes with this already in it??
    Yeah. Shouldn't be an issue. Once it's cured, you shouldn't have the issue again.
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

+ Reply to Thread

Thread Information

Users Browsing this Thread

There are currently 1 users browsing this thread. (0 members and 1 guests)

     

Similar Threads

  1. Mirror gloss black+Midnight clear
    By peter61 in forum Powder Coating Questions
    Replies: 4
    Last Post: 10-19-2008, 06:40 PM
  2. high gloss clear
    By boston_jake01 in forum Powder Coating Questions
    Replies: 5
    Last Post: 01-23-2007, 10:08 PM
  3. HFSD vrs. Super High Gloss Clear?
    By mtnbiker in forum Powder Coating Questions
    Replies: 3
    Last Post: 09-08-2006, 09:49 PM
  4. low gloss clear, does caswell have it
    By corybarta in forum Powder Coating Questions
    Replies: 0
    Last Post: 02-18-2006, 07:57 PM
  5. Differences between HFSD Clear and Super High Gloss Clear
    By sab0276 in forum Powder Coating Questions
    Replies: 2
    Last Post: 01-05-2006, 03:08 PM

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts

Search Engine Friendly URLs by vBSEO 3.5.0 RC1 PL1