Default small Nickel plating job-any takers?

I have a tub faucet that I am intersted in getting plated in a satin Nickel finish. It is currently polished brass, and has a "pitts" in it. It is an expensive unit, and I would like to plate it instead of replacing, if possible.

Thanks

btw, it is about 8" long or so, and about 6.5" deep. I can get exact measurements
Reply With Quote
  #2 (permalink)  
Old 05-14-2004, 04:51 PM
Amateur Metal Finisher
 
Join Date: Dec 2003
Posts: 203
fxstcguy98 is on a distinguished road
Default

where are you located? Do you want chrome over the satin nickle?
Reply With Quote
  #3 (permalink)  
Old 05-14-2004, 10:43 PM
Newbie
 
Join Date: May 2004
Posts: 13
y2khardtop
Default

near Charlotte NC.

No, I want satin nickel over polished brass. The photo is an example of my fixture, but mine is currently brass!

Thanks
Reply With Quote
  #4 (permalink)  
Old 05-15-2004, 07:29 PM
Amateur Metal Finisher
 
Join Date: Dec 2003
Posts: 203
fxstcguy98 is on a distinguished road
Default

OK
I am in Columbus OH. You might want to find someone closer, the shipping costs will make it expensive.
Thanks
Reply With Quote
  #5 (permalink)  
Old 06-07-2004, 08:07 PM
Amateur Metal Finisher
 
Join Date: Feb 2004
Posts: 109
dagobert
Default Still needing it done?

Have you gotten the faucet replated yet? If not, how bad is the pitting? As the old saying goes, "you can't polish a turd", but if it's not too eaten up, I'd be willing to give it a shot. To get a satin finish, I can glass-bead blast it and then copper plate it, then nickel plate it without a lot of polishing inbetween. That should give it the texture it sounds like you are describing. Let me know here if you are interested. I'm in Columbia, TN (just south of Nashville).

Jay
Reply With Quote
  #6 (permalink)  
Old 11-09-2004, 11:33 AM
Newbie
 
Join Date: Sep 2004
Location: Florida
Posts: 28
wop1969
Default

I can repair and nickel plate the item you have.

I'm located in Florida and if you still need and are interested please go to my website and see my gallery of work I have done. There is also contact information there so you can get ahold of me.
http://www.leveinc.com
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Gold Plating and Nickel plating tzmandevil Electroplating Questions 2 09-16-2005 09:11 AM
Nickel bath inexplicably quits plating jackf Electroplating Questions 5 01-25-2005 09:55 PM
Nickel plating wanted Carmel N.Y. area (Small Job) cappi Services Offered/Wanted 0 05-06-2004 01:48 PM
boron plating on electroplated Nickel jackf Electroplating Questions 0 03-29-2004 01:41 AM
Need Nickel Plating (small job) in NYC (could use mail) higginsjr Services Offered/Wanted 0 03-10-2004 10:14 AM


All times are GMT -4. The time now is 12:59 AM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.