Default Nickel or chrome plating of fishing lures

Would anyone be interested in nickel plating or chrome plating some fishing lures. They are 4 oz lures.....I cast them along the ocean shore. As lure is reeled in the shine gets dull and eventually wears off. The lures cost roughly $4.00 each.....want to know if I could get some of my old lures made like new with something that won't wear off so quickly...Any suggestions ....Thanks Greg
Reply With Quote
  #2 (permalink)  
Old 01-13-2005, 04:35 PM
warchild's Avatar
Amateur Metal Finisher
 
Join Date: Feb 2003
Location: Seymour,Tn.
Posts: 147
warchild
Default

I mite could plate them for you. send me a pic and size of them. my e-mail---> warchild_007@hotmail.com
__________________
WARCHILD
Reply With Quote
  #3 (permalink)  
Old 07-10-2005, 04:57 PM
customandsound
Guest
 
Posts: n/a
Default

warchild what part of w.v you in? i got some little thing i don't want to polish for the car that would look good chromed ..
Reply With Quote
  #4 (permalink)  
Old 07-16-2005, 06:05 AM
fly fly is offline
Amateur Metal Finisher
 
Join Date: Jun 2005
Location: beaumont misssissippi
Posts: 310
fly will become famous soon enoughfly will become famous soon enough
Default

If you want to give me a try I could do the job but I live in mississippi, the shipping is probably more than the lure cost. One thing you could try is a polish, the lure's are probably made of stainless. If they are chrome you could try very fine steel-wool (0000) to bring back the shine.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Plating Problem grey finish from chrome plating tshirah Electroplating Questions 2 08-13-2005 12:08 AM
Differet copper plating questions, plus copy chrome/ nickel? krsimulis Electroplating Questions 1 07-26-2004 12:25 AM
GOLD PLATING FISHING LURES lureman Electroplating Questions 1 07-24-2003 02:09 PM
Plating Fishing Lures kjbdnb Electroplating Questions 1 05-29-2003 11:01 PM
Chrome, Nickel or copy chrome? dwthomas Electroplating Questions 1 02-15-2003 01:49 PM


All times are GMT -4. The time now is 02:29 PM.


Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.