I have a set of wrestling belt plates that I would like to have plated. They are made of cast zinc and I need them gold plated. I am in North Carolina and if you can do the job please contact me at keithkeever@charter.net
|
|
|||
|
I just joined Caswell and didn't notice a reply to your post. So even though it's been awhile since u posted... I hope this helps. You cannot plate over zinc. It must be removed by soaking the part in a mixture of 50% muriatic acid and water. Soak until all the zinc has been dissolved and proceed as if plating raw steel. Since your piece is ALL zinc, it cannot be plated.
|
|
||||
|
It can be plated if you first plate with our Flash Copper solution, which works as effectively as cyanide based copper plates, without the dangerous chemicals. Flash Copper plates very well over zinc.
You can then plate with nickel, then gold.
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
|
|||
|
__________________
Fred Luhn Goldies Gold Plating Service New York http://www.goldiesplating.com 718-529-6655 Voice/Fax |
|
||||
|
You're welcome
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Gold Plating and Nickel plating | tzmandevil | Electroplating Questions | 2 | 09-16-2005 09:11 AM |
| Nickel bath inexplicably quits plating | jackf | Electroplating Questions | 5 | 01-25-2005 09:55 PM |
| Plating and high heat | chromo | Electroplating Questions | 1 | 01-29-2003 01:15 AM |
| plating and size power? | chromo | Electroplating Questions | 7 | 01-18-2003 02:52 AM |
| Electroless Krome plating Q's | chcarver | Electroplating Questions | 1 | 10-10-2002 10:00 PM |