Hello,
I have a brass PR-24 Police Baton that I would like to have permanently "anodized". I understand it is not possible to "anodize" brass, but I would like to shine it one more time, them maybe laquer it so it will look awesome for life. Anybody interested in taking on this job? Here is a visual on the baton:
|
|
||||
|
Not that I wouldn't like to earn your money but I don't know if you would be happy with a clear coat in the long term. Not very many clear coats do well on bare metal. Have you tried a good carnuba wax or better yet Zoop Seal. It's suppose to be good for two years in the weather.
http://www.caswellplating.com/buffs/zoopseal.html |
|
||||
|
We had recommended that he spray the part with VHT Clear Lacquer, which has given us excellent results over the years and was designed for brass and copper work.
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
![]() |