Default Copper/Nickel Bath for electroforming

Would anyone here with a tank setup be willing to try a copper electroforming job? I'm thinking of electroforming some small bowls instead of having them spun or hammered. I can mail the wax model and provide the conductive paint. This is kind of an experiment in enamelling on my part, so if it doesn't work that well all I'm out is some money. I'd be curious to try it in nickel as well, but I'm not sure how thick nickel will plate.
Reply With Quote
  #2 (permalink)  
Old 11-05-2005, 03:17 AM
fly fly is offline
Amateur Metal Finisher
 
Join Date: Jun 2005
Location: beaumont misssissippi
Posts: 310
fly will become famous soon enoughfly will become famous soon enough
Default Re: Copper/Nickel Bath for electroforming

What size or the bowls and how many. I might be able to help you if you want to try it out.
Reply With Quote
  #3 (permalink)  
Old 11-05-2005, 10:12 AM
Newbie
 
Join Date: Dec 2004
Posts: 9
topspinner
Default Re: Copper/Nickel Bath for electroforming

Two bowls maybe 4in. or 5in. in diameter and 4 in. deep.
Reply With Quote
  #4 (permalink)  
Old 11-05-2005, 09:01 PM
fly fly is offline
Amateur Metal Finisher
 
Join Date: Jun 2005
Location: beaumont misssissippi
Posts: 310
fly will become famous soon enoughfly will become famous soon enough
Default Re: Copper/Nickel Bath for electroforming

Lets give it a try see what it will do. Just ship it to me and I will start on it as I can because I plate on the side, so it might take a little time. You can ship it by mail or ups its up to you.

Ship to: Shane Hesterman
P.o. box 302 / 906 4th st.
Beaumont ms, 39423
(601) 549-6914
Reply With Quote
  #5 (permalink)  
Old 11-05-2005, 10:20 PM
Newbie
 
Join Date: Dec 2004
Posts: 9
topspinner
Default Re: Copper/Nickel Bath for electroforming

You're actually ahead of me on this. I have to order a few more items before I can turn the bowl, so It'll be some time yet. I'm interested in having you try it, so I'll drop you a note in the mail or through this system when the bowls are ready.
Reply With Quote
  #6 (permalink)  
Old 11-06-2005, 12:03 AM
fly fly is offline
Amateur Metal Finisher
 
Join Date: Jun 2005
Location: beaumont misssissippi
Posts: 310
fly will become famous soon enoughfly will become famous soon enough
Default Re: Copper/Nickel Bath for electroforming

Ok, if you can try to have a place to hang the bowl from if you can, if not I will find a spot.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Lead contamination of nickel bath? hakelly Electroplating Questions 2 12-21-2003 05:58 PM
Copper Bath SDE Electroplating Questions 1 12-21-2003 02:06 PM
Dull black parts when taken out of nickel bath. neil Electroplating Questions 1 08-04-2003 11:05 AM
I think I ruined my nickel bath Tad Anderson Electroplating Questions 1 05-24-2003 11:28 PM
Did I mess up my nickel bath? Shevalik Electroplating Questions 3 07-25-2002 12:36 PM


All times are GMT -4. The time now is 07:25 PM.


Powered by vBulletin® Version 3.7.4
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0
Copyright © Caswell Inc.