im not in NY but i can help .
you can reach me at powerplating@yahoo.com http://www.geocities.com/powerplating/
__________________
Jim Eaton |
|
|||
|
Hi! we are located 45 minutes from upstate on the NJ side, not far from I-87. We do polishing, plating and much much more for a fraction of the price. 973-395-0770....call us, and ask any questions you might have! Good luck,
Perfectmetalpolishing@yahoo.com |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Removing small scratches from Chrome | mlust | Metal Polishing Questions | 5 | 07-30-2008 02:39 PM |
| Copy Chrome on engine parts and plastic, alot of can I's | cgworth | Copy Chrome Kit Customers Only | 3 | 08-29-2005 12:38 PM |
| Small Parts Plating in or around San Francisco, CA | ckm | Services Offered/Wanted | 0 | 05-17-2005 05:18 PM |
| Copy Chrome Start-up | Elitefisherman | Electroplating Questions | 10 | 04-18-2004 04:24 AM |
| Detail chrome plating for show parts!! | GOD12A | Electroplating Questions | 0 | 01-11-2004 11:08 PM |