    i want to make a bigger anno tank than my 5 gallon. i want to go to a 20 gallon. one a good container for it. links would be nice. also a way to put an permanent temp reader in the tank also are the lead plates a neccessary to have or can i use something else as a ground. im gonna buy some aluminum tubbing and coil it up and put one in two of the corners and pump ice water thru to get my tank so i can hopefully use it this summer. Also is there any type of temp mod that i can get that i can set the temp and it will turn the ice water pump on and off as per needed. 20 gallon might be over shooting it as something that will be big enough to fit all of a paintball gun parts in so i dont have to do two runs..