new posts

  • Stripper

    Some of the newer parts my customers are getting from the factory is Nickel Plated. What stripper would be best to be used to remove this coating so it can be anodized the color of their choice?

  • #2
    Are the Parts Aluminum ?
    --
    Jason Vanderbroek
    315 946 1213 x116
    www.caswellplating.com

    Comment


    • #3
      yes. All parts i deal with are aluminum

      Comment


      • #4
        you would need our B929 Nickel Stripper, Then our Metal X copper Stripper (assuming there is a copper layer under the nickel)
        --
        Jason Vanderbroek
        315 946 1213 x116
        www.caswellplating.com