    Hello can anyone tell me why my sealer gets chalky and leaves a white chalky film on my parts

  • #2
    What temp were you using it at ? What type of bath container ?
    --
    Jason Vanderbroek
    315 946 1213 x116
    www.caswellplating.com

    Comment


    • #3
      180-185 in a hdpe container

      Comment


      • #4
        That chalk is a precipitate of some kind. What is the pH of the tank?
        Process control doesn't give you good quality, it gives you consistent quality.
        Good quality comes from consistently doing the right things.

        Process control systems for Anodizers
        If a post helps you out LIKE the post
        I'm not an Amateur Metal Finisher. I've just been around the industry for a dozen years or so helping and consulting when and where I can.

        Comment


        • #5
          Last I checked it was around 6.5