    I have not done any anodizing in several years and everything I anodize in the past was 6061 aluminum. I will be machining several pieces out of 7075 aluminum and plan to anodize them. What differences can I expect when anodizing 7075?
    Thanks, Jim

  • #2
    Cut your ano time to 75% of that of 6061. Be sure to desmut also as it tends to smut more than 6061 due to the zinc content.