    I know we have the sticky page in the forum but it is missing 4 colors. I sent an email to tech support but they haven't answered and it has been a week. Does any body have the values for:

    Green JAS
    Camo Brown
    Gold N
    Orange 2B

    Thanks

    Ian

  • #2
    I sent these to you a week or so, I will re send them now.
    --
    Jason Vanderbroek
    315 946 1213 x116
    www.caswellplating.com

    Comment


    • #3
      I haven't received anything in my email since I made the support ticket on Dec 7th.

      Comment


      • #4
        I apologize, not sure what happened there. Here they are

        Green JAS = 5.0 +- .5

        Camo Brown = 6.0 +- .3

        Gold N = 4.5 +- .5

        Orange 2B = 6.0 +- .5
        --