    Hey there,

    Being new to this game ive started setting up my equipment and all that left is the PS. I will be doing my motorcycle wheels which ive calcualted to need around 700W supply though i want to future proof with as little cost as possible as its just a hobby.
    The largest thing i can ever see myself anodizing is a car rim which estimating requiring 1000W

    The question is, what do you guys recommend doing to achieve around 18v constant current supply. Ive seen regaular PS's with addons to allow constant current but cant find any for my power needs.
    Basic knowledge of small electronics tells me that 2 PS's is a terrible idea but does that apply here also?

    Thanks in advance