  • Replacement buckets for Anodizing...Help!

    Hello - Purchased Caswell Anodizing kit many years ago. I need to replace the 6 Gallon buckets and lever-lock lids. Anyone know a supplier for these buckets? I'm thinking of going with 10 gallon buckets if they are available. Thanks!

  • #2
    I would stay away from the Caswell buckets. I have a new kit and the bottom of the degreaser bucket split at 175 degrees f. My heat source is a plastic commercial sous vide heater suspended from the side about six inches from the bottom. What a mess!