    I've been doing research on the anodizing bath. My 6 quarts of battery acid weighs 18 pounds. At 33/67 percent that means that I have about 6 pounds of acid and 12 pounds of water. If I follow Caswell's directions of 1:3 that means I need to add 4.5 gallons of water. That will yield a solution of around 12%

    Is my math right, and if so, is a 12% solution what I'm looking for? I always thought 15% was closer.
    Last edited by [email protected]; 03-16-2021, 11:00 PM.

  • #2
    That will work just fine.
    --