Tried my 1st couple parts. Followed the manual. The parts look perfect olive drab as what dye was used when their wet. When dry it turns a purplish chameleon color until it's wetted again then back to the correct color. Thoughts?
Welcome To The Caswell Inc Forums - The Place To Be For Metal Finishing Enthusiasts!
We notice that you are not currently registered on our site, or are not logged in. Registration is FREE and allows you to post questions on our forums, post pictures, access Technical Support, place orders for products and much, much more! Why not take a moment and register? Just click the Register Link above.