    replied
    i had a bunch of information, but none of it was really important in that i figured out why some of it was occuring.

    my problem before was i didn't know how much current or voltage was necessary for a certain amount of square footage. i have since figured out the mathematical problems, in that using 4.5 amps a sq. foot will always need at most 11.5 volts (being the PAR), and the current and resistance varies depending on the surface area of the part.

    i've narrowed my problem down to the resistance/CV problem with the power supplies.

    Leave a comment:


  • NeoMoses
    replied
    umm, I read this earlier and thought it had more information... did you figure out your problem?

    Leave a comment:


  • potsked
    replied
    see above

    Leave a comment:


  • potsked
    started a topic Appropriate power supplies

    Appropriate power supplies

    see this thread for my current problem (no pun intended! HAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHA HAAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAAHHAHAHAHAHAHAH AHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAH AHAHAAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAAHHAHAHAHAHA HAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHA HAHAHAHAAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAAHHAHAHAH AHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAH AHAHAHAHAHAAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAAHHAHA HAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHA HAHAHAHAHAHAHAAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAHAAHH AHAHAHAHAHAHAHA

    I AM SO FUNNY!

    no really go here

    http://www.caswellplating.com/bbs/viewtopic.php?t=1543