  • #16
    I'll be looking forward to seeing your dyeing post.

    I use alligator clips too, clear of the electrolyte of course. They work fine if they have teeth to bite into the wire, Wiggling them a little after clipping them on, so that the teeth dig into the wire is a good practice. Using clips with strong springs also helps.

    Comment


    • #17
      My problem was small cheap aligator clips, apparently they lacked the required spring power. Even after working them on the wire, they didn't seem to work as well as possible.

      Comment


      • #18
        NeoMoses, I now have the eddy current thickness gauge back.