    i have no clue how anodizing is done. i'v recently got into pc and would like to do some anodizing. what "home" kit can i buy and basicly i'd like to know how to do it.. yes i will be searching and reading, just needed a beginner's coarse... thanks

  • #2
    Caswell's 'home kits' are availablehere.

    The best source for info for a beginner is the LCD anodizing instructions, available here.