    Hey Guys,

    Would regular tap water run through a water filter system (Reverse Osmosis system) work in place of all require distilled water in a anodizing setup?

    Randy

  • #2
    Yes, as long as its working propperly. http://www.caswellplating.com/kits/ro_unit.html
    Easttex

    Comment