what type of a anode do I use for Anodizing?
Announcement
Collapse
No announcement yet.
anode for anodizing?
Collapse
X
-
Re: anode for anodizing?
It's not really an anode in an anodizing set-up, but you can use a sheet of lead.
We sell a higher quality, lead-antimony based sheet that gives better results.
See http://www.caswellplating.com/access.htm#Anodes--
Mike Caswell
Caswell Inc
http://www.caswellplating.com