    UV reactive dye would make it visible in the dark with the aid of a blacklight

    Comment


    • #17
      caswell im interested in flourescent green and orange also. thanks

      Comment


      • #18
        other dye source

        I have heard of some people using fabric dyes for anodizing. they are organic, like regular aluminum dyes, but some fade rather easily.

        I also do tie dye as a hobby and found craft stores sell fabric dye in powder form. Also, Daharma sells a lot of dyes and has a wide variety of colors. Check their web site.

        The problem with true florescent dyes is the particle size is large, you will have problems getting enough dye in to the small pores to do a good job.
        The florescent dies listed at Caswell are not really responding to u.v. light,
        but take the appearance of glowing.