This is my first time anodizing.
My parts do not look like take the dye.
I wonder how much should i add into the water. I add about 10g for my 1L tank.
I have no idea how long it takes for the dye process.
Please help.
thanks,
My parts do not look like take the dye.
I wonder how much should i add into the water. I add about 10g for my 1L tank.
I have no idea how long it takes for the dye process.
Please help.
thanks,