the flames where cut out with a vinyl cutter. Have a cutter. i think it was 3mil vinyl. (same stuff you would find on a vechile lettering or strickers)
once you place it down your down nothing you can do. anything you use to postion it. will mostlikly mess with the dying and leave blemish.
and the marker is a brass eagle Rainmaker.
www.rainman229.com
Announcement
Collapse
No announcement yet.
just showing off alittle
Collapse
X
-
Very nice. I like the style of flames. Did you cut them yourself? What material? Did you use backer positioning material?
BTW, what marker is that from? My son and I are scratching our heads on this one.
Leave a comment:
-
just showing off alittle
little note on removing the glue. wd40 after sealing and then hit it with 3m adhicive remover after about a 1/2 hour. comes right off with no elwo greeceTags: None