why do some parts cook in the acid different than other pieces? I did 2 pieces at once ,same material ,cleaning time ,etc.when it came to the color stage they came out different. one took well, the other didn\'t.any help would be greatful.
Announcement
Collapse
No announcement yet.
anodizing
Collapse
X
-
Re: anodizing
There\'s a variety of reasons, but we need more information to help you.
Please use our PRS system to post a problem report - http://www.caswellplating.com/support.htm--
Mike Caswell