  • Distilled Water?

    New Question. The Deluxe Anodizing kit comes with the Reveres Osmosis System. Every thing I read states Distilled water. Do I still need Distilled water? Or is the filtered water ok.

    Thank you for any input.

  • #2
    reverse osm. water will work just as well as distilled. Just don't use tap water.

    Comment


    • #3
      Thank you