reverse osm. water will work just as well as distilled. Just don't use tap water.
Leave a comment:
-
Distilled Water?
New Question. The Deluxe Anodizing kit comes with the Reveres Osmosis System. Every thing I read states Distilled water. Do I still need Distilled water? Or is the filtered water ok.
Thank you for any input.Tags: None