I am a student trying to anodize some AL 6061-T6 for research. My intentions are to do a FPL pretreatment and then Phosphoric Acid Anodization.
I am reading from text that the FPL etch bath needs a compistion of 15.0 parts FeS0(4) 37 parts H(2)SO(4) and 48 parts H(2)O and the PAA to have 100 g/L H(3)PO(4).
I am interested in the following questions:
1. Is FPL and PAA safe enough to do in a lab (fume hood is accesible)?
2. If 1. is yes, is there a kit with specified solutions above?
3. If no kit is available with those solutions, can I buy a kit and then use my own solutions obtained elsewhere?
I appreciate all the help...thank you.
I am reading from text that the FPL etch bath needs a compistion of 15.0 parts FeS0(4) 37 parts H(2)SO(4) and 48 parts H(2)O and the PAA to have 100 g/L H(3)PO(4).
I am interested in the following questions:
1. Is FPL and PAA safe enough to do in a lab (fume hood is accesible)?
2. If 1. is yes, is there a kit with specified solutions above?
3. If no kit is available with those solutions, can I buy a kit and then use my own solutions obtained elsewhere?
I appreciate all the help...thank you.