Re: What do you use for storing all ur solutions?
I have started an album on the anodize tanks and setups I have gone through since I started. I haven't got all the pics to current but close. Check it out. Maybe you will see something that will help you.
Announcement
Collapse
No announcement yet.
What do you use for storing all ur solutions?
Collapse
X
-
Re: What do you use for storing all ur solutions?
Many home repair places have HDPE white buckets in 2 to 6 gallon sizes with lids. The lids are a little hard to get on and off but they work well. Mark contents with marker.
Leave a comment:
-
What do you use for storing all ur solutions?
Well, I was thinking about just getting a bunch of rubbermaid containers to use for everything, what do you use for the anodize bath? for the dyes? ano stripper? well basicly everything?
Thanks for the helpTags: None