  • The amazing Ano-Tester!

    Okay...no so amazing but definately one of the handiest bits of kit I've thrown together in a few minutes.

    All thats needed is a LED, battery and some metal prongs (in this case a couple aluminium rivets). Its a great way to check if you've anodised something especially when like us we do a lot of clear.

    Anyways - just thought I would share
    Attached Files

  • #2
    Re: The amazing Ano-Tester!

    Excellent idea! I LOVE the simplicity of it.

    Any chance of a photo of it's gizzards?
    --
    Mike Caswell
    Caswell Inc
    http://www.caswellplating.com
    Need Support? Visit our online support section at http://support.caswellplating.com

    Comment


    • #3
      Re: The amazing Ano-Tester!

      There isn't anything to it - just completes a circuit.

      Just grab a battery - resistor - LED - break the circuit with some pins of some sort - then wire the second pin back to the battery. We put a little switch to turn it off when needed but its not really.

      The scary thing is how conductive your hands are when you cross the pins - watch out for grounding those big PSU's
      Attached Files

      Comment


      • #4
        Re: The amazing Ano-Tester!

        Hmmm.....why didnt you just use a multimeter?
        not flaming, just curious.

        Comment


        • #5
          Re: The amazing Ano-Tester!

          This just seems faster. Instead of spending time reading a display all you have to do is touch an item. Light on, bad, light off, good.