    hi folks, i have some microphone bodies with a extreemly fine thread i need anodised, and i was wondering if the process would clog the threads?

    what are your thoughts?

    the thread size is approx 65tpi

    thanks in advance

    matt

  • #2
    Re: Thickness of anodising

    Why risk it when you can use plugs, Mask-it or tapes to shield the threads?
    --
    Mike Caswell
    Caswell Inc
    http://www.caswellplating.com
    Need Support? Visit our online support section at http://support.caswellplating.com

    Comment


    • #3
      Re: Thickness of anodising

      The anodize will not clog the threads. It may tighten them up a little. Most threads cut in production are at least a class II. Sometimes a class III. If you feel some slack in the threads now, you should be ok. SS

      Comment


      • #4
        Re: Thickness of anodising

        it is an extreemly tight and fine thread. we will see, i will ask the anodising guys advice, he will have a better idea of his processes.

        thankyou
        matt