my black dyes have been coming out pretty pale recently and i think it may be the dye. I've checked the Ph and ajusted it to 5.5 -6.0, but the part still comes out pale. Is there any way to check to see how much dye is left in the tank.
Announcement
Collapse
No announcement yet.
Dye problems
Collapse
X
-
Re: Dye problems
I use quite a few different colors and haven't used any particular color enough to deplete the dye. Maybe one of the other guys can help on that question. If your running 20% acid, the pale color could be caused from too thin a coating and /or pore size too large to hold enough dye for a dark black. SSLast edited by sswee; 12-22-2005, 12:05 PM.