    What is the absolute best conditions to anodize at, using 12 amps per square foot. All of the variables. Temp, Acid content, whatever else you can think of.
    thanks.
    texsol
    New User
    Last edited by texsol; 12-22-2005, 04:56 PM. Reason: spelling.

  • #2
    Re: What is the absolute best

    Originally posted by texsol
    What is the absolute best conditions to anodize at, using 12 amps per square foot. All of the variables. Temp, Acid content, whatever else you can think of.
    thanks.
    720 Rule
    Temp. 60 - 72 degrees. I prefer low 60's. Slows dissolution.
    5% acid - 3:1 distilled water : battery electrolyte
    Tank agitation is very important.