new posts

  • hulk30
    replied
    Re: rocket science

    thank again for the infos
    i will watch the video for sure
    thank again guys

    Leave a comment:


  • mcaswell
    replied
    Anodize Video

    I have JUST today finished the LCD Anodizing video.

    I hope to put it on the web as a streaming video later today at www.moonrakers.com/weblcd.mov

    It will be available on VHS and DVD shortly

    I think this should solve most of your problems

    Mike
    Last edited by mcaswell; 02-26-2006, 07:26 AM.

    Leave a comment:


  • sswee
    replied
    Re: rocket science

    I think it would be much easier to master than the English language.
    If you read the LCD anodizing instructions and understand the basics of what anodize is, it helps.
    There is some math to figure SA (surface area) and CD (current density), so you know how much current to use for a part. A basic understanding of DC electricity is helpful. The step by step instructions are clear and if followed there is no reason you cannot anodize.
    Parts made of billet aluminum are no problem to anodize. Cast parts will range from easy, difficult, to can't do.
    The biggest problem with parts like valve covers and intakes is their power requirements to do the large amount of SA and a tank large enough to dissipate the heat that will be generated. Most carbs. are made of cast mixes that do not anodize with the exception of the base plates.
    A well organized setup could use as little as a 10' x 10' area but like most things the more room the better.
    If you have any other questions or I was not clear in my answer, just let me know.
    SS

    Leave a comment:


  • hulk30
    started a topic rocket science

    rocket science

    i don t know nothing about anodizing
    it could be a good business opportunity for my new shop
    but the more i read about it seem very complicate
    i d ont know by seeing it,i will understand but reading about it,what i job
    like i said before english is not my first language so i guess try to understand the process don t help me
    can i anodize aluminium valve cover, intake , carburetor etc
    if i buy a kit is it simple to understand what i thinking is a step by step process for rookie like me
    like anything else i guess practice make perfect
    do i need lot of room to operate ,