Re: Which green dye looks the best?
When dyed to full color, they may look similar at a glance. The SCG is more of a green (shamrock green), the AEN leans slightly to a forest green with a dark tint to it.
http://forum.caswellplating.com/phot...to/757/cat/520
Hopr this helps