    replied
    No, they won't fade.

    Just follow the instructions in the manual and you should get good results.

    Leave a comment:


  • dancollinsjr
    started a topic Anodizing Dye - Light Fastness/Fading

    Anodizing Dye - Light Fastness/Fading

    Do your dyes fade in outdoor applications? I will be using your blue dye(DYEB9), any special tricks/tips to miminize fading, such as, which sealant, room temp. or boiling is recommended.

    Thanks, Dan