i recently got the gold dye and have tried anodizing a few pieces with it, the problem i have is that i've only gotten 2 pieces to actually look gold in color. i did 5 pieces at the same time and all the other ones came out more of an orange color than gold. i even reanodized the other pieces and left them in the dye for less time and the same thing happens.