i just tried the lt sealant and did it by the directions and it stripped all the dye off my piece, it was only in there a few minutes. after spending hours getting my pieces ready and anodized then this happens kinda made me pretty mad
Announcement
Collapse
No announcement yet.
lt sealant
Collapse
X
-
Hmmm, it doesn't do this by design. It's a sealant not a stripper and is a commercial grade sealing product (used by large anodizing shops all over the world)
If you can provide some more details to us, using our support section, we'll help you figure out exactly what went wrong.--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
-
Can you please send us a picture of this? We've not heard of this happening before. PLease send to [email protected]