    replied
    Re: Acid for anodizing

    Battery acid is mostly, but not 100% sulfuric acid. Sulfuric acid is 100% sulfuric acid.

    We recommend battery acid for our kits and processes. Some people may find sulfuric acid works best in other products. It\'s really up to you to experiment.

    Leave a comment:


  • dburg507
    replied
    Re: Re: Acid for anodizing

    caswell wrote:
    It should all be virtually the same.

    Semi-related note: Some people try to use sulfuric acid instead of battery acid....it\'s not the same concentration and doesn\'t work out of the bottle.
    Hello,
    Hope you don\'t mind if I add on to this thread, but what you said caught my eye about sulfuric acid not working out of the box. Can you give a little more detail on that. Reason being we currently use battery acid but my partner seems to think we should switch to sulfuric acid. I did some research and I\'m not sure if I want to use that stuff. If can tell me what the pro\'s and con\'s are that would be great.

    Thanks in advance

    Leave a comment:


  • mcaswell
    replied
    Re: Plug n plate kit for bathroom faucets ?

    1.26 baum

    Leave a comment:


  • ketanjajal
    replied
    Re: Re: Acid for anodizing

    Can you tell me the exact concentration by volume/weight or Molarity. I need this since I have limited supplier from whom i can buy.

    thanks

    Ketan

    caswell wrote:
    It should all be virtually the same.

    Semi-related note: Some people try to use sulfuric acid instead of battery acid....it's not the same concentration and doesn't work out of the bottle.

    Leave a comment:


  • mcaswell
    replied
    Re: Acid for anodizing

    It should all be virtually the same.

    Semi-related note: Some people try to use sulfuric acid instead of battery acid....it's not the same concentration and doesn't work out of the bottle.

    Leave a comment:


  • desert_roamer
    started a topic Acid for anodizing

    Acid for anodizing

    Is automotive battery acid the same mixture (1/3 acid, 2/3 water) from all sources? The plating manual recommends getting it from NAPA auto stores for use in anodizing, but I have some from a different source. Does it matter as long as its automotive battery acid?