Bill,
First find out what you a trying to plate!!!
Later,
Tim
Announcement
Collapse
No announcement yet.
Plug n Plate chrome
Collapse
X
-
Plug n Plate chrome
I'm attempting to plate a small metal bracket - not sure of the material but it's conductive. My problem is that, following instructions, the wand and solution only pruduce a dark, dull gray finish which easily buffs off. I've tried reversing the wires from the power supply, but no difference.
Any help appreciated.