  • mcaswell
    replied
    You'd need some Silvaspray and a small gold immersion kit. See http://www.caswellplating.com/kits/

    Leave a comment:


  • lureman
    started a topic GOLD PLATING FISHING LURES

    GOLD PLATING FISHING LURES

    Hi all,
    I currently produce fishing lures with a painted finish.These lures are made of polyurethane so don't conduct electricty.I would like to incorporate a goldplated model into my range of lures.I have dabbled with vacuum metalizing but I have to send them away to have this process done.I thought a hobby goldplating kit maybe the way to go.My question is would it and how much to set up?