Announcement
Collapse
No announcement yet.
Electroless Krome question
Collapse
X
-
Electroless Krome question
I just got your Electroless Krome kit and I'm going to use it to "Krome" some brass pieces. The question I have is, after I electroless Krome my brass pieces, can I then gold plate them with my existing cyanide based pen plater that I already have?
Will gold plate directly onto a "Krome" finish?
Thanks for any info.Tags: None