    Re: flexibility of nickle/chrome/gold plate

    Nickle and chrome are fairly hard metals and would likely crack if flexed.

    Gold, being softer, is less likely to crack.

    Leave a comment:


  • studuff
    started a topic flexibility of nickle/chrome/gold plate

    flexibility of nickle/chrome/gold plate

    I was wondering how the adherence of the above plating would be affected if they were used on something like a coil spring - something that will be flexing a certain amount. Would the plate be likely to crack or flake off?